dear friends,
can you please suggest me the best possible technique to perform Stellite powder coating BY PTA welding on hard materials like monel & inconel? i found difficulty and components often got rejected..please give me your best suggestions.

Regards.
 
Replies continue below

Recommended for you

Different methods and techniques apply to different underlying alloys. Have a look at the attachment, which should help you specify your query.

I work with valves in exotic alloys at alloy-valves.com. This is me on Twitter and LinkedIn. Let's connect!
 
 http://files.engineering.com/getfile.aspx?folder=dc50a97a-678c-4b0b-b313-398c7959a24f&file=Stellite.pdf
Why were the components rejected? Micro fracturing?
 