Anyone has experience with very heavy hardfacing by PTA? layer material - Stellite 6; substrate - mild steel. The height of the deposit is to be 20mm. The width of the deposit is to be 22mm and the length of the deposit is 400mm. This deposit will not be supported on the sides. Each pass will give me approx 3mm build up. I will need to do 7 runs to get the desired height of 20mm.
Would appreciate info re the multi passes, pre-heats, potential cracking etc.