Feb 15, 2016 #1 xuanthien Mechanical Joined Mar 27, 2013 Messages 17 Location VN Dear Sir, Pls advice welding consumable to weld repair_Buttering and hardfacing of Ni-Cr-Mo Material.
Dear Sir, Pls advice welding consumable to weld repair_Buttering and hardfacing of Ni-Cr-Mo Material.
Feb 15, 2016 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Not enough information. What is the specific alloy? What hardfacing are you considering - Stellite? Upvote 0 Downvote
Feb 17, 2016 #3 EdStainless Materials Joined May 20, 2004 Messages 16,357 Location Waukesha WI USA Will the base metal require PWHT after buttering? What is the specific base alloy? What is the service? What potential hardfacing are you looking at? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote