I am looking for protective coatings for LCD applications. These coatings have to be able to withstand the following two post processing steps: (1) Sputter overcoat of SiO2 and ITO where temperatures reach as high as 300 C IN VACUUM for about 5 minutes, (2) ITO etching step where the coating gets exposed to 30% HCl for about 1 minute.