I have a w27x114lb x 240"l I-beam with a 12"w x 240"l 1"t plate on top and a 12"w x 240"l x .625"t plate on bottom. The reason for the plates was to achieve the section modulus needed and to meet required existing heights and safety factor. What I am unsure of is appropriate welding practice to simulate these plates being part of the I-beam. We were originally going to bevel and seam weld all interface edges all around. I am worried about tempering the I-beam when introducing that much heat. So how much of a weld do I need. Can it be stitch welded 1 foot every foot or some other variant?
Thanks for the impute
Dallas
only in a steel mill.
Thanks for the impute
Dallas
only in a steel mill.