I have two potential weld repairs.
Repair No. 1: I have welded a Category A joint with the SAW welding process. It was determined by UT that there is linear indication about 1/8 in. under the service and about 2 in. long. I was considering repairing it with FCAW, however since it is Category A, per UG-84(i)(1), I would have to run a production impact test plate using the FCAW process. Is this a correct interpretation? Also, the vessel thickness is approx. 8 3/8 in. thick. Do I have to weld this thickness for the production impact test plate or can I use a smaller thickness, such as 1.5 in., test plate?
Repair No. 2: There are small repairs on base metal of this vessel on a bevel preparation. The bevel preparation on one vessel will be welded to another bevel preparation on another vessel to create a Category B weld joint, which would require a production impact test plate at the time of welding this joint per UG-84(i1). Would I need to perform a production impact test plate to perform these repairs on a bevel preparation prior to it becoming a Category B joint? (Note: I understand that I can use the production impact test plate, if needed, for Repair No. 1 for this repair, if required).
Repair No. 1: I have welded a Category A joint with the SAW welding process. It was determined by UT that there is linear indication about 1/8 in. under the service and about 2 in. long. I was considering repairing it with FCAW, however since it is Category A, per UG-84(i)(1), I would have to run a production impact test plate using the FCAW process. Is this a correct interpretation? Also, the vessel thickness is approx. 8 3/8 in. thick. Do I have to weld this thickness for the production impact test plate or can I use a smaller thickness, such as 1.5 in., test plate?
Repair No. 2: There are small repairs on base metal of this vessel on a bevel preparation. The bevel preparation on one vessel will be welded to another bevel preparation on another vessel to create a Category B weld joint, which would require a production impact test plate at the time of welding this joint per UG-84(i1). Would I need to perform a production impact test plate to perform these repairs on a bevel preparation prior to it becoming a Category B joint? (Note: I understand that I can use the production impact test plate, if needed, for Repair No. 1 for this repair, if required).