Hey fellas,
I'm trying to qualify a new corrosion resistance overlay procedure per QW-453. I will be doing it on 1" plate in the 1G position with the GTAW process.
My question is, will an individual whom is certified to weld with GTAW in 6G be able to use this procedure to weld in all positions, as long as he stays within the other essential variables?
I'm trying to qualify a new corrosion resistance overlay procedure per QW-453. I will be doing it on 1" plate in the 1G position with the GTAW process.