I'm trying to weld pieces of 6061 tube together which are .032" thick, 2.5" wide.
I just got a Miller Dynasty 200DX and I am still learning how to use it. I'm using a/c, 150amps, but I'm not sure of the other settings I should have setup on the machine to make a good weld. It just wants to burn through the pipe wall no matter how delicate I am with the foot control, it goes from not melting to melting the wall and cutting back from the edge, how can I weld this joint effectively?
If anyone knows about my welder and could help me I'd really appreciate it, I'm trying to get this project completed.
~Will
what should argon be flowing at?
what amperage should I run?
I'm using 3/32 filler wire
what about all those frequency and intial slope settings?
I'm confused!
I just got a Miller Dynasty 200DX and I am still learning how to use it. I'm using a/c, 150amps, but I'm not sure of the other settings I should have setup on the machine to make a good weld. It just wants to burn through the pipe wall no matter how delicate I am with the foot control, it goes from not melting to melting the wall and cutting back from the edge, how can I weld this joint effectively?
If anyone knows about my welder and could help me I'd really appreciate it, I'm trying to get this project completed.
~Will
what should argon be flowing at?
what amperage should I run?
I'm using 3/32 filler wire
what about all those frequency and intial slope settings?
I'm confused!