eetm
Electrical
- Nov 26, 2002
- 5
We currently package 16 and 32 oz HDPE bottles that are either flourinated treated or not. The bottles are made by one manufacturer using the same molds. We send out about 1/3 of these to get treated. We have no problems with sealing the caps on the non treated bottle but have problems with the treated bottles. The caps have a sheet of aluminum embedded and after the cap is torqued to the bottle it passes through an induction sealer. The induction sealer has to be run at full power output for the treated bottles and runs at a much lower setting for non-treated bottles.
I'm looking for a solution to this problem or reasons why this is happening. Thx in advance.
I'm looking for a solution to this problem or reasons why this is happening. Thx in advance.