I am using a Material 1.4404 in my analysis.
Along with the Youngs Modulus,density and poisson ratio, I am also defining Johnson Cook(also strain rate dependency) Plastic hardening parameters:
Following are the values used:
A = 514
B = 514
C = 0.042
n = 0.508
m = 0.533
strain rate = 0.001
After running the simulation,I am getting the following error:
1)THE STRAIN INCREMENT HAS EXCEEDED FIFTY TIMES THE STRAIN TO CAUSE FIRST YIELD AT 44 POINTS
I have been trying to analyse it, but could not find any solution till now.
Waiting for some update from anyone
Thanks in advance!
I am using a Material 1.4404 in my analysis.
Along with the Youngs Modulus,density and poisson ratio, I am also defining Johnson Cook(also strain rate dependency) Plastic hardening parameters:
Following are the values used:
A = 514
B = 514
C = 0.042
n = 0.508
m = 0.533
strain rate = 0.001
After running the simulation,I am getting the following error:
1)THE STRAIN INCREMENT HAS EXCEEDED FIFTY TIMES THE STRAIN TO CAUSE FIRST YIELD AT 44 POINTS
I have been trying to analyse it, but could not find any solution till now.
Waiting for some update from anyone