I have 0.250" thick carbon steel pressure vessel.
Original max pressure rating 90 PSI 320 deg. F
Actual operating 30 PSI at 270 deg F
Vessel has pitting approx nickel size diameter to 0.125"
deep. 1.Can metal be added such as bead welding to rebuild
or fill the pits as a temporary patch, permanant repair, or not at all?
2.If individual doing repair is certified would the vessel need recertification and or pressure test?
Original max pressure rating 90 PSI 320 deg. F
Actual operating 30 PSI at 270 deg F
Vessel has pitting approx nickel size diameter to 0.125"
deep. 1.Can metal be added such as bead welding to rebuild
or fill the pits as a temporary patch, permanant repair, or not at all?
2.If individual doing repair is certified would the vessel need recertification and or pressure test?