Hi,
We have a Production Separator with the following data:
Design Code ANCC PNR (Italian Standard)
Position: Horizontal
Stress Relieved: Yes
Radiographed: Whole Joints
Shell—Material Fe E-45-UNI 5869 (Original Thickness 32)
Size—Nominal ID, mm 4154
Length Base Line to Base Line, mm 15000
Design—Pressure, psi 256
Operating Press, psi ±150
Design Temperature, oC 80
Operating Temp, oC ~ 80
Widely Scattered Pitting & Metal Loss found at the Separator Bottom (Minimum Recorded Thickness,
mm 10.36)
Is it better to repair, after Preparing the Surface, by only Weld Filling all Points ≤ 7.64 mm? or shall we line the Whole Affected Area Using Patch Plates? In case we have to weld patch plates, is it mandatory to use the same materials of the separator plates, or we can propose alternatives like ASTM A283 Gr. C?
The original WPS/PQR of the said Separator is missing. So, do you think that we can use an approved 6G-SMAW-Pipe using E7016 & E7018-G and API 5L Gr. X52 pipe WPS/PQR for the qualification of the welders who are going to perform the job?
The last point, I seek your advice concerning the repair welding procedure as long as the plates of the vessel have previously been heat treated.
Thank you for your usual cooperation.
Best regards,
We have a Production Separator with the following data:
Design Code ANCC PNR (Italian Standard)
Position: Horizontal
Stress Relieved: Yes
Radiographed: Whole Joints
Shell—Material Fe E-45-UNI 5869 (Original Thickness 32)
Size—Nominal ID, mm 4154
Length Base Line to Base Line, mm 15000
Design—Pressure, psi 256
Operating Press, psi ±150
Design Temperature, oC 80
Operating Temp, oC ~ 80
Widely Scattered Pitting & Metal Loss found at the Separator Bottom (Minimum Recorded Thickness,
mm 10.36)
Is it better to repair, after Preparing the Surface, by only Weld Filling all Points ≤ 7.64 mm? or shall we line the Whole Affected Area Using Patch Plates? In case we have to weld patch plates, is it mandatory to use the same materials of the separator plates, or we can propose alternatives like ASTM A283 Gr. C?
The original WPS/PQR of the said Separator is missing. So, do you think that we can use an approved 6G-SMAW-Pipe using E7016 & E7018-G and API 5L Gr. X52 pipe WPS/PQR for the qualification of the welders who are going to perform the job?
The last point, I seek your advice concerning the repair welding procedure as long as the plates of the vessel have previously been heat treated.
Thank you for your usual cooperation.
Best regards,