Sep 16, 2011 #1 tightrope Industrial Joined Sep 16, 2011 Messages 4 Location TT i am a first timer to dis forum and would like to know how to pressure test 420ft of 1\2 stainless steel pipinp
i am a first timer to dis forum and would like to know how to pressure test 420ft of 1\2 stainless steel pipinp
Sep 16, 2011 #2 MikeHalloran Mechanical Joined Aug 29, 2003 Messages 14,450 Location US First figure out how much pressure it's supposed to hold. Mike Halloran Pembroke Pines, FL, USA Upvote 0 Downvote
Sep 17, 2011 Thread starter #3 tightrope Industrial Joined Sep 16, 2011 Messages 4 Location TT 150 psi Upvote 0 Downvote
Sep 18, 2011 #4 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Use treated water (no chlorides), rated fittings, pipe cap and a pump. Upvote 0 Downvote
Sep 18, 2011 #5 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Oh yes, hold for 10 minutes at pressure and check for leaks. Drain and dry. Upvote 0 Downvote
Sep 18, 2011 Thread starter #6 tightrope Industrial Joined Sep 16, 2011 Messages 4 Location TT thank u very much would give it a try and c how it will turn out and let u know Upvote 0 Downvote
Sep 22, 2011 Thread starter #7 tightrope Industrial Joined Sep 16, 2011 Messages 4 Location TT been asked to install 300ft of 2" P.V.C piping how do i charge the costmer for this job Upvote 0 Downvote
Sep 23, 2011 #8 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US tightrope; Find another line of work. Upvote 0 Downvote
Sep 26, 2011 #9 EagerLearner Chemical Joined Sep 22, 2011 Messages 27 Location BN What is a Material test certificate? Do we need this each time we order a std 316SS orifice plate? Can we have one certificate to represent a shipment of orifice plates of different sizes, class and thickness? Upvote 0 Downvote
What is a Material test certificate? Do we need this each time we order a std 316SS orifice plate? Can we have one certificate to represent a shipment of orifice plates of different sizes, class and thickness?
Sep 27, 2011 #10 MikeHalloran Mechanical Joined Aug 29, 2003 Messages 14,450 Location US EagerLearner, please repost that as a new message, Red Flag this one, and ask that it be removed. Thank you for your courtesy. Mike Halloran Pembroke Pines, FL, USA Upvote 0 Downvote
EagerLearner, please repost that as a new message, Red Flag this one, and ask that it be removed. Thank you for your courtesy. Mike Halloran Pembroke Pines, FL, USA