Hi,
I am currently work on two different cases where I need to reduce pressure in a seawater pipe.
1. 10", flow rate 690m3/h, pressure drop 4,5 barg
2. 10", flow rate 1600m3/h, pressure drop 9 barg
Today we have installed orifices but these are creating cavitation and the vibration and noice is of the scale.
We are considering to install control valves but as we are then talking about titanium the cost will be a major issue.
So my question is, is there anybody that have experienced similar problems. I am looking for an alternative to the orifice. Something less costly than the control valve.
Any ideas would highly appreciated.
Tom
I am currently work on two different cases where I need to reduce pressure in a seawater pipe.
1. 10", flow rate 690m3/h, pressure drop 4,5 barg
2. 10", flow rate 1600m3/h, pressure drop 9 barg
Today we have installed orifices but these are creating cavitation and the vibration and noice is of the scale.
We are considering to install control valves but as we are then talking about titanium the cost will be a major issue.
So my question is, is there anybody that have experienced similar problems. I am looking for an alternative to the orifice. Something less costly than the control valve.
Any ideas would highly appreciated.