Hello,
We are looking at retaining an ABS injection molded faceplate on a small sheet metal drawer. The sheet metal drawer is only .030 Aluminum so snap features aren't really an option and must avoid screws. We have 4 bosses protruding from the faceplate that will pass through holes in the drawer. The two options we are exploring are heat staking the bosses into rivet heads or possibly using press nuts. I've seen many applications for heat staking but don't know much else about the process (e.g. temperature to properly "flow" the plastic without it melting execessively and making a mess) and how to go about obtaining tooling. The 4 bosses are 3/16" OD with a 3/32 core. Press nuts are commonly used on low cost metal shafting (garden cart axles, toys, etc) and seem simpler than heat staking.
My questions are:
Does anyone in this group have some expertise in heat staking they could share with me?
Has anyone used press nuts on ABS? I'm a little concerned about creep or the nut digging into the plastic and subsequent loosening of the faceplate over time.
I apologize in advance for the long winded post but wanted to provide as much information as possible up front.
Thanks,
Kyle
We are looking at retaining an ABS injection molded faceplate on a small sheet metal drawer. The sheet metal drawer is only .030 Aluminum so snap features aren't really an option and must avoid screws. We have 4 bosses protruding from the faceplate that will pass through holes in the drawer. The two options we are exploring are heat staking the bosses into rivet heads or possibly using press nuts. I've seen many applications for heat staking but don't know much else about the process (e.g. temperature to properly "flow" the plastic without it melting execessively and making a mess) and how to go about obtaining tooling. The 4 bosses are 3/16" OD with a 3/32 core. Press nuts are commonly used on low cost metal shafting (garden cart axles, toys, etc) and seem simpler than heat staking.
My questions are:
Does anyone in this group have some expertise in heat staking they could share with me?
Has anyone used press nuts on ABS? I'm a little concerned about creep or the nut digging into the plastic and subsequent loosening of the faceplate over time.
I apologize in advance for the long winded post but wanted to provide as much information as possible up front.
Thanks,
Kyle