canwesteng
Structural
As part of a retrofit of a building, we will be saw cutting concrete, which will leave rebar exposed. My concern is the exposed rebar will start to corrode and eventually cause decay of the whole slab. Does anyone have experience in this type of situation, and what might be recommended to preserve the bar?