Jun 4, 2015 #1 zaki29 Mechanical Joined Mar 6, 2015 Messages 6 Location EG I prepared wps according to pqr, preheat temperature is not stated in pqr, so I write it in wps NA, but the Client need to add it in the WPS WHAT can i do? wps and pqr according to asmi ix weather temperature is about 31°C to 38°C
I prepared wps according to pqr, preheat temperature is not stated in pqr, so I write it in wps NA, but the Client need to add it in the WPS WHAT can i do? wps and pqr according to asmi ix weather temperature is about 31°C to 38°C
Jun 4, 2015 1 #2 blaqesmith Materials Joined Jul 13, 2013 Messages 45 Location JP Decrease in Pre heat is essential variable so you should note temperature value. Upvote 0 Downvote
Jun 4, 2015 Thread starter #3 zaki29 Mechanical Joined Mar 6, 2015 Messages 6 Location EG can I state it ambient temperature Upvote 0 Downvote
Jun 4, 2015 #4 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US If you did not apply preheat, use the ambient temperature condition on the PQR for preheat prior to welding. Upvote 0 Downvote
If you did not apply preheat, use the ambient temperature condition on the PQR for preheat prior to welding.