in our company's internal standard until now a preheat temperature of 300°C for welding P5 piping is required.
Now a disucssion is started weather a temperature range of 250-300°C is also acceptable.
In every case PWHT is required so I don't worry over much about remaining martensite.
Also Asme B31.3 requires an even lower preheat temperature.

Does anybody know of a standard (api, nace,..) requiring at least 300°C preheat temperature?
Pipes are used in corrosive (mainly sulfidation) refinery service.

Thank you for your advice.

Daniel Breyer
Inspection Engineer

 
Replies continue below

Recommended for you

For SA 335 P5 alloy steel, a proper minimum preheat temperature is 200-220 deg C. Having a preheat of 300 deg C is of little benefit and places you up against the interpass temperature limit. What was the basis for my recommendation? - ASME B31.1 for P-No 5B materials, which is conservative.
 