Hello,

I am trying to predict erosion rate per year for slurry piping.
However, I am not sure if it is possilbe to use formula or otherwise there is any specific software available.
Could somebody please help me out?

Thank you.

Regards
 
Replies continue below

Recommended for you

Do a web search for, "Erosion in elbows in hydrocarbon production systems: Review document" Prepared by TÜV NEL Limited for the Health and Safety Executive, 2003 RESEARCH REPORT 115
 