I am trying to predict erosion rate per year for slurry piping.
However, I am not sure if it is possilbe to use formula or otherwise there is any specific software available.
Could somebody please help me out?
Do a web search for, "Erosion in elbows in hydrocarbon production systems: Review document" Prepared by TÜV NEL Limited for the Health and Safety Executive, 2003 RESEARCH REPORT 115