Got a small precast circle supporting brick veneer. About a 6' span. Load is about 300 lbs/ft. For design sakes, I am assuming all the brick will be on the arch, no brick arching action.

They want to do 4 pieces of precast, split in the quarter locations. My analysis shows moment obviously. What are your thoughts of doing a field epoxy anchor to join them together?

BTW, I am also going to ask them to do 2 piece with a false joint, and actual joint at the 3 and 9 position. They already have some similar arches with same span, so not sure why needs to be 4 pieces.

Thoughts?
 
Replies continue below

Recommended for you

Check your epoxy material for long-term loading. Many polymers are focussed on resisting short-term loading and creep can be noticeable.
 
JStructsteel said:
My analysis shows moment obviously.

It's not obvious. You have a circular arch. People have been building these as compression only structures - some without any mortar at all - for thousands of years. A uniformly loaded semi-circular or even segmental arch shouldn't need the connection you're talking about.

Here's a BIA Tech note on unreinforced, semi-circular brick arches. Might be worth a read.
 
Agree with pham. maybe it needs to be temporarily shored during construction but this is a pure compression arch.
 
PhamENG, thanks. I thought about that. I can make sure its all mortared in with the brick around the perimeter to give it that support. Im still going to do a pin of some kind at the joint I think to give it alignment and out of plane redundancy.
 