Hi all,

I was curious as to what the suggested pre-treatment options are for Al Alloys prior to powdercoating? We primarily use 6061-T6/T6511 and 5052-H32, and I currently am calling out a 5 stage Iron Phosphate pre-treatment but upon doing some research I am seeing a lot along the lines of a Chromate conversion coating. What are the pros and cons of both? I assume Hexavalent Chromium would be more expensive due to the toxic issues with it, but I also see non-Hexavalent containing Chromate conversions; what does this entail? these parts are for structural members of vacuum systems, and while they aren't going to be seeing a constant salt spray or anything they do have the potential to be operated outside for the majority of its use near marine environments.
 
Replies continue below

Recommended for you

The Powder Coating Institute lists several pre-treatment options: Chrome phosphate, Hexavalent chromate, Trivalent chromate and some titanium and zirconium chemistry with a polymer. To get better direction for your application, contact one of the treatment chemistry suppliers such as Henkel.
 
You should use a hexavalent chromium free pretreatment. Some options include Alodine from Henkel, Iridite from MacDermid, and Gardobond and Oxsilan from Chemetall.
 