I am looking for a pre-preg material that is suitable for use in jet fuel. I also need it to have constant electrical properties from one batch to the next. Is there anyone who can help me out?

Jeff
 
Replies continue below

Recommended for you

Any prepreg material you use will not offer long term impermeability to jet fuel all by itself. A rubber based coating like PRC or similar fuel selant has to be used to serve as a barrior.

The Prepreg material you choose should have a resin content of upwards of 35 % to provide a smooth glossy surface for the fuel sealant compound.

Prepreg Glass : NB321 7781 ( Newport Adhesives and Composites)
Prepreg Carbon Fabric : NB 321 3K 70P ( Newport )

Please let me know if you need further details.

Thanks,

AK
 