I have a building built in 1966. The floor slabs are concrete 16" thick with 12" diameter tubes cast in (like todays hollow core planks). My question is what do you think these 12" diameter tubes are made of? Did they have PVC back then? Steel or iron tubes seem like a lot of dead load.
 
Replies continue below

Recommended for you


pylko,

We ran into a situation similar to this a few years back and the tubes used there were transite pipe sections. I wonder if those you encountered might be transite also?

David
 
Wasn't transite used for water pipes years ago?
 