Aug 10, 2017 #1 mulz Mechanical Joined Jul 15, 2015 Messages 18 Location SA Dear, What is the pre-heating temperature in the latest edition of asme b31.3 coz we are dealing with welding of piping whose diameter is 16'',cs, sch.80.. Thanks mulz
Dear, What is the pre-heating temperature in the latest edition of asme b31.3 coz we are dealing with welding of piping whose diameter is 16'',cs, sch.80.. Thanks mulz
Aug 10, 2017 4 #2 DekDee Petroleum Joined Mar 12, 2012 Messages 1,324 Location PH If you are working to the latest edition of B31.3 then you had better purchase a copy. Upvote 0 Downvote
Aug 10, 2017 #3 XL83NL Mechanical Joined Mar 3, 2011 Messages 3,121 Location NL DD's reply is the best youll get to your question. Upvote 0 Downvote
Aug 10, 2017 #4 david339933 Industrial Joined Jun 15, 2011 Messages 1,204 Location CA When you do get a copy, check out Table 330.1.1 Upvote 0 Downvote
Aug 12, 2017 Thread starter #5 mulz Mechanical Joined Jul 15, 2015 Messages 18 Location SA Thanks to all of you. Upvote 0 Downvote