Is preheat maintenance an essestial variable when you are not exceding the maximum interpass temperature?
My GTAW P8 WPS states in QW-403 60 degree min preheat temp / 350 degree max interpass temp / preheat maintenance none.
we will be welding 347ss overlay on existing 347ss overlay to build up for machining RTJ flange grooves and are required to preheat at 250 degrees.
would this wps need to be requalified or is this acceptable?
My GTAW P8 WPS states in QW-403 60 degree min preheat temp / 350 degree max interpass temp / preheat maintenance none.
we will be welding 347ss overlay on existing 347ss overlay to build up for machining RTJ flange grooves and are required to preheat at 250 degrees.
would this wps need to be requalified or is this acceptable?