Hi

If we have a PRQ for two different base metals, say P#1 to P#8, does this PRQ also qualify welding P#1 to P#1 and P#8 to P#8.

In practise welding the same base metals would use a different filler and other WPS/PRQ. Using the above WPS/PRQ would be a but odd, but could you?
 
Replies continue below

Recommended for you

C'mon Kevin,
As a fellow Kiwi a little bit disappointed you asked a pretty basic question that is clearly identified in QW 424.1.
As I got hammered into me many times - read the code, then read it again, then ask questions,
Cheers,
Shane
 
Thanks Shane

We do read the code, but sometimes we can not see the wood for the trees
 