Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Powerfloating waffle slab

Status
Not open for further replies.

JacksPanic

Structural
Feb 23, 2012
42
Has anyone had any experience with powerfloating a waffle slab? the slab is 450mm thick and the topping above the voidformer is 125mm thick. Is 125mm not too thin to powerfloat? i'll appreciate your comments.
 
Replies continue below

Recommended for you

What would make it too thin to powerfloat, JacksPanic? I can't think of a single reason why a five inch thick slab could not be powerfloated, but maybe you will convince me otherwise.

BA
 
I cannot convince you otherwise because I agree with you. The builder seems to doubt it though. He says the top will end up being "wavy" over the void formers and ribs.
 
The only reason you could get a "wavy" surface is if the ribs are not adequately compacted, thus allowing for plastic settlement. Make sure the ribs are vibrated thoroughly, then the finishing should be routine.
 
Status
Not open for further replies.

Part and Inventory Search