I'm looking at making some prototype powdered metal parts in house which is something I do not have experience with. I'm looking at doing some research on different solid lubricant add mixtures to powdered metal parts which is the reason I am not just having this farmed out. The part is a simple ring as shown in the drawing below. I added a 3 degree draft angle to hopefully simplify the process. I have some 90/10 pre-mix 100 mesh powder order. I plan on placing the pressed part in a vessel purged with argon in an oven with a type K thermocouple to sinter. My question is regarding the die design.
1. Will a two piece top an bottom design with 3 degree tapered walls suffice? My hope is the the part fall out after pressing without needing any sort of ejectors. Is this realistic?
2. I plan on cold pressing via manual operation with a 20 ton shop press, nothing close to a production environment. The cross sectional area for the part is only 0.38in^2 so theoretically I could achieve up to 105,000psi?
3. I want the part about as dense as practical so what pressing pressure should I consider?
4. Is there a rule of thumb on the fill volume vs pressed volume to use when designing the die? I suppose this is easy to figure out for a before and after pressing density but I don't know what is realistic for the pressed density.
5. What shrinkage rate to expect after sintering?
6. From what I have gathered the sintering schedule for something like this would be around 1,500F for 30 minutes. Does this sound right?
1. Will a two piece top an bottom design with 3 degree tapered walls suffice? My hope is the the part fall out after pressing without needing any sort of ejectors. Is this realistic?
2. I plan on cold pressing via manual operation with a 20 ton shop press, nothing close to a production environment. The cross sectional area for the part is only 0.38in^2 so theoretically I could achieve up to 105,000psi?
3. I want the part about as dense as practical so what pressing pressure should I consider?
4. Is there a rule of thumb on the fill volume vs pressed volume to use when designing the die? I suppose this is easy to figure out for a before and after pressing density but I don't know what is realistic for the pressed density.
5. What shrinkage rate to expect after sintering?
6. From what I have gathered the sintering schedule for something like this would be around 1,500F for 30 minutes. Does this sound right?
![URL]](https://res.cloudinary.com/engtips/image/fetch/w_800,c_lfill,q_auto,f_auto,g_faces:center/[URL unfurl="true"]http://www.practicalmachinist.com/vb/attachments/f38/187162d1482955159-die-design-powdered-metal-part-seal_ring_drawing.jpg[/URL])