Nov 18, 2011 #1 engr2GW Petroleum Joined Nov 7, 2010 Messages 308 Location US Hi all, Please, I'm looking for the material or name of the insulation material that is used to wrap around a weld in order to slow down coling and increase the amount of Hydrogen that leaves the weld. Any help please will be appreciated!!!
Hi all, Please, I'm looking for the material or name of the insulation material that is used to wrap around a weld in order to slow down coling and increase the amount of Hydrogen that leaves the weld. Any help please will be appreciated!!!
Nov 18, 2011 1 #2 weldtek Materials Joined Feb 12, 2005 Messages 897 Location US There are many, but, ceramic fiber works well. Kaowool or equal. Upvote 0 Downvote
Nov 18, 2011 #3 kingnero Mechanical Joined Aug 15, 2009 Messages 1,783 Location BE Vermiculite (although you can't really wrap that around something)... Upvote 0 Downvote