Hi Everyone,

If vessel clips are welded to the reactor that requires PWHT. Do we have to PWHT the entire reactor or just localized area?. What section of ASME section VIII Div. 1 specify the requirements for this particular case.

Thank you very much in advance for your help.

azn4850
 
Replies continue below

Recommended for you

Don't know the code section, but you shold be able to do a local PWHT-unless the vessel is 304 SS, etc. You might also be able to do a "temper bead" weld.
 