Dear Team,
I have to weld a combination of materials as mentioned below.
1. ASTM A213 T11 to T22 (ASME Section IX P No. 4 to P5A)
2. ASTM A213 T22 to T22 (P No. 5A to 5A)
3. ASTM A213 T22 to T91 (P No. 5A to P15E)
Can anyone suggest a suitable PWHT temperature which can allow furnace heating of all combinations together.
I have to weld a combination of materials as mentioned below.
1. ASTM A213 T11 to T22 (ASME Section IX P No. 4 to P5A)
2. ASTM A213 T22 to T22 (P No. 5A to 5A)
3. ASTM A213 T22 to T91 (P No. 5A to P15E)
Can anyone suggest a suitable PWHT temperature which can allow furnace heating of all combinations together.