What are the effects of several (5 times) heat treatments on a tubesheet material SA336 F22 Cl3 (with Inconel cladding )and tubes SA 213 T22 material.
Tubesheet is PWHT-ed in the furnace after welding the Inconel cladding.After this 4 local heat treatments are executed due to repairs.
After first repair a test is done and the hardness on the HAZ of tube was after one cycle 193 HV10 after 2 cycles 221Hv10.
In the ASME code any restriction of heat treatment cycles is made. Can this be accepted ?