Oranda,
Same as the effect on RC members plus about 10% but no one thinks about it for RC members .
The normal procedure would be to provide a pour strip in the slab between the 2 codes allowing the compression from the PT to get into the concrete. Then closely spaced reinfrocement (same as RC, about 200 centers) should be provided to give crack control for shrinkage etc.