I am modelling a plastic part in ANSYS 12.2
I applied mesh,connections, forces and suports.
I solved and got solution
I applied a froce of 1200N
Max stress was at 206 MPa
UTS of material is at 135 MPa
I need to find the force (which should be less then 1200N) at which the part will fail, any way other then trail and error, to find that out?
Thanks
I applied mesh,connections, forces and suports.
I solved and got solution
I applied a froce of 1200N
Max stress was at 206 MPa
UTS of material is at 135 MPa
I need to find the force (which should be less then 1200N) at which the part will fail, any way other then trail and error, to find that out?