I am currently trying to match the results that were obtained in an Instron machine within COSMOS Premium 2008 and have had some success. I am able to match the force necessary to reach the plasticity point within 5.7% but the data after that is not correct (See attached image)
The study is a nonlinear static study and to mimmick the instron compression machine I have applied a reference geometry restraint that compresses the model constantly. I then used the resultant force result to extract the force for every time step and plotted this in excel.
Is there a way to obtain the correct force after the model has reached the plasticity point? The type of material is 6061-T6 aluminum and the data for this was obtained direct from cosmos material library. I would appreciate any insight into this issue because I have exhausted all other resources.
Thanks in advance.
The study is a nonlinear static study and to mimmick the instron compression machine I have applied a reference geometry restraint that compresses the model constantly. I then used the resultant force result to extract the force for every time step and plotted this in excel.
Is there a way to obtain the correct force after the model has reached the plasticity point? The type of material is 6061-T6 aluminum and the data for this was obtained direct from cosmos material library. I would appreciate any insight into this issue because I have exhausted all other resources.