Hi ALL:
I am working with gold plating, over Ni, on Cu... standard stuff. But, I ran into an engineer who insists that gold plating is porous, or more exactly, gold itself is porous. As far as I know, that is not the case. But, he insists that since Hg gets absorbed by gold: the Hg moves into the pores in the gold (his explanation), and actually can move through the gold. He also insists that since Hg is a large atom (true) that other atoms like Ni and Iron can move through the pores in the gold, or gold plating, since a large atom, like Hg can.
On thin gold plating, without a Ni substrate (or suitable substrate, and barriers), you can see the copper, "migrate", over extended time, through the gold plating. He says, the copper atoms travel through the pores in the gold, to the surface of the gold plating, which is wrong. Maybe someone can comment, because he doesn't believe me... I'm not a materials guy.
Regards
I am working with gold plating, over Ni, on Cu... standard stuff. But, I ran into an engineer who insists that gold plating is porous, or more exactly, gold itself is porous. As far as I know, that is not the case. But, he insists that since Hg gets absorbed by gold: the Hg moves into the pores in the gold (his explanation), and actually can move through the gold. He also insists that since Hg is a large atom (true) that other atoms like Ni and Iron can move through the pores in the gold, or gold plating, since a large atom, like Hg can.
On thin gold plating, without a Ni substrate (or suitable substrate, and barriers), you can see the copper, "migrate", over extended time, through the gold plating. He says, the copper atoms travel through the pores in the gold, to the surface of the gold plating, which is wrong. Maybe someone can comment, because he doesn't believe me... I'm not a materials guy.
Regards