thread330-217250
The above thread references Nitrogen solubility in CA6NM. We are having porosity issues in casting with thinner walls (0.5"). I am having our heat tested for nitrogen content. In the mean time can any one comment about what percentage of Nitrogen would cause porosity in CA6Nm castings? Also, if the nitrogen in the heat is higher than desired, is there any way to remove this nitrogen during melting?
Thank you,
--------------------------------------
There is always some thing better out there...
Mahadhatu
The above thread references Nitrogen solubility in CA6NM. We are having porosity issues in casting with thinner walls (0.5"). I am having our heat tested for nitrogen content. In the mean time can any one comment about what percentage of Nitrogen would cause porosity in CA6Nm castings? Also, if the nitrogen in the heat is higher than desired, is there any way to remove this nitrogen during melting?
Thank you,
--------------------------------------
There is always some thing better out there...
Mahadhatu