I have an application in which I have to filter ammonia at -50 to -70 F. I have concerns in which these temperatures are below the Tg of Polymers such as Polypropylene, Polyester and Cellulose which are used as filter media. Would building a differential pressure across the media by the flow of the fluid cause any issues.
 
Replies continue below

Recommended for you

You would have to consider the design taking the pressure and material properties at that temperature into account.

Can you get tensile strength, impact, fatigue, elongation and modulus figures for the fibres at those temperatures.

HDPE has relatively good low temperature properties.

Regards
pat pprimmer@acay.com.au
eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Filter Media made of expanded PTFE (Trade name Gore-Tex) should do your job very well. Contact Gore for more information.
 