About a year ago we bought a nice food processor, which features a steady rest pintle on the power shaft. The cover has a mating plastic bearing. They appear to be the same polymer.

It worked fine until yesterday, when the machine welded up. I had trouble breaking the assy apart. I finally coaxed it apart, and the pintle was found to be heat damaged. I restored it to working order, and, by giving it a shot of non stick spray on every setup, I got it to perform as usual.

What happened? I think the two plastics were identical, like acetal-acetal or nylon-nylon. I will suggest to the mfr to use acetal-nylon as suggested by DuPont. Any other suggestions?
 
Replies continue below

Recommended for you

Acetal nylon is a great combination, and hard to beat in such applications. My only reservation might be the temperature resistance of acetal. If you need higher temperatures, try nylon polyester

Regards
pat pprimmer@acay.com.au
eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor