Hi All,

First time posting on this forum, so please bare with me if I'm posting this thread in the wrong forum.

I am working on a project for work and I am finding a real hard to time to find an adhesive that would stick Polyetheylene to Polycarbonate. I know there are some adhesives that are out in the market however they are flammable and therefore cannot be used in our manufacturing environment.

I need your expertise. Please advise.

Thank you for response in advance.

Steve
 
Steve
Try reposting this in the forum728 I think you will get more response there. The polyethylene is going to be the tough one.
B.E.

You are judged not by what you know, but by what you can do.
 
to STEVO123

Sorry for you but POLYETHYLENE, POLYPROPYLENE and PTFE have no adhesive, not at all. The only possibility is mechanical connection
 