Jun 27, 2005 #1 brakemeister Automotive Joined Aug 15, 2002 Messages 41 Location US Does anybody know what Poisson's Ratio is for 430 Stainless? I have checked Matweb.com and can't seem to find it.
Does anybody know what Poisson's Ratio is for 430 Stainless? I have checked Matweb.com and can't seem to find it.
Jun 27, 2005 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US The information in the file below is on 430 SS. Poisson's ratio is reported to be 0.30 at 20 deg C. http://www.australwright.com.au/DataSheets/Alloys/Stainless Steels/430 SS.pdf Upvote 0 Downvote
The information in the file below is on 430 SS. Poisson's ratio is reported to be 0.30 at 20 deg C. http://www.australwright.com.au/DataSheets/Alloys/Stainless Steels/430 SS.pdf
Jun 27, 2005 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Seems like I copied a bad link. Try here; http://www.australwright.com.au/DataSheets/ Upvote 0 Downvote