Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Please identify this bolt, european? 2

Status
Not open for further replies.

pacesetter

Mechanical
Sep 22, 2006
18
Hi, can you please identify this bolt from the attached photo. Interpolating the width across the flats results in a measurement of 1.80 inches.

Thanks a bunch,
Jeff
 
Replies continue below

Recommended for you

The L7 label on the bolt is to identify it as grade L7 according to ASTM A 320/A 320M Standard Specification for Alloy/Steel Bolting Materials for Low-Temperature Service. This grade has a minimum yield strength of 105 ksi, and a minimum tensile strength of 125 ksi.

You can obtain this specification from ASTM International:


The interlocking hexagons are the head identification symbol for KPF (a Korean company), the bolt's manufacturer. They are included on page 98 of MIL-HDBK-57C LISTING OF FASTENER MANUFACTURER’S IDENTIFICATION SYMBOLS, which is available at ASSIST: