Aug 5, 2022 #1 RVinothkumar Mechanical Joined Apr 16, 2021 Messages 31 Location IN Please explain, why basic electrodes are baked and why cellulosic electrodes are not baked? What is the reason behind baking oven and holding oven?
Please explain, why basic electrodes are baked and why cellulosic electrodes are not baked? What is the reason behind baking oven and holding oven?
Aug 15, 2022 #2 LittleInch Petroleum Joined Mar 27, 2013 Messages 22,906 Location GB You should ask in the welding forum or maybe do a bit of searching? but something to do with low hydrogen / water content. Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote