Please explain, why basic electrode

Status
Not open for further replies.

RVinothkumar

Mechanical
Joined
Apr 16, 2021
Messages
31
Location
IN
Please explain, why basic electrodes are baked and why cellulosic electrodes are not baked? What is the reason behind baking oven and holding oven?
 
You should ask in the welding forum or maybe do a bit of searching?

but something to do with low hydrogen / water content.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 