flyforever85
New member
I'm trying to compare the FE results with a hand calculation but I'm not having great luck yet.
I have a plate, 300 mm x 300 mm, (aluminum 72,000 MPa, v=.33), thickness 3 mm. An homogeneous pressure of 0.005 MPa is applied all over the plate. THe plate is fixed at every edge.
The FEM model gives me a max deflection of 1.81 mm at the center of the plate while a formula from Bruhn gives me a max deflection of 0.92 mm (the formula is wmax = (alpha x q x a^4)/(E x t^3) where q is the pressure, a is the edge length. alpha depends on the boundary condition and for a fixed edge it's 0.0438
Thogths?
I have a plate, 300 mm x 300 mm, (aluminum 72,000 MPa, v=.33), thickness 3 mm. An homogeneous pressure of 0.005 MPa is applied all over the plate. THe plate is fixed at every edge.
The FEM model gives me a max deflection of 1.81 mm at the center of the plate while a formula from Bruhn gives me a max deflection of 0.92 mm (the formula is wmax = (alpha x q x a^4)/(E x t^3) where q is the pressure, a is the edge length. alpha depends on the boundary condition and for a fixed edge it's 0.0438
Thogths?