Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

plastic for casting pattern 1

Status
Not open for further replies.

kenre

Mechanical
Joined
May 23, 2005
Messages
300
What are the best choices for a machinable plastic for use as a casting pattern, used in sand castings.?

Wood is commom, but i would like something that is a little more robust.


Was told it couldnt be done, so
i went and did it!
 
When a more robust pattern is required for sandcasting, it is common to use metal faced wood patterns or all metal patterns.
 
You can use epoxy patterns. You can also use polyurethane foam(commonly thermocole) material.

If you can give a little more information it will be helpful.

Chocolates,men,coffee: are somethings liked better rich!!
(noticed in a coffee shop)
 
The patterns are small, approx 6 in Sq, and have quite a bit of detail in them. I would like to use metal but machining them will take forever, there being done on a homebuilt cnc mill.

I will be starting with petrobond sand molds and move onto a phenolic bonded sand if i need higher volumes.






Was told it couldnt be done, so
i went and did it!
 
You can use as mentioned earlier,araldite patterns,they are long lasting,easy to work with and economical.

Chocolates,men,coffee: are somethings liked better rich!!
(noticed in a coffee shop)
 
arunmao, By epoxy (araldite being a trade name) are you saying to take a mold from the orgiginal wood pattern or machining from a block? ive never seen a solid block of epoxy.

My experience in epoxy is for laying up molds using carbon, kevlar and fibregrass.






Was told it couldnt be done, so
i went and did it!
 
Yes you are right. We often cast a solid block into near desired shape and then work on it to finish. This will be faster than metal patterns.

If you need one,send along a drawing I shall get one for you free,!

Chocolates,men,coffee: are somethings liked better rich!!
(noticed in a coffee shop)
 
Thankyou, interesting way to do it. do you use certain types of epoxy?

Are there any plastics that are also suitable? eg, nylon, acetel, as these are easy enough to source. I would be suprised if plastics arent used!




Was told it couldnt be done, so
i went and did it!
 
There can be others who might have tried,but I have been working with araldite for nearly 20 years.

Chocolates,men,coffee: are somethings liked better rich!!
(noticed in a coffee shop)
 
Something like Araldite AY 103 with an appropriate hardener should be castable in blocks.
 