Aug 5, 2004 #1 rodneyb Mechanical Joined Jun 26, 2001 Messages 30 Location US I read it is bad practice to put countersunk screws in plastic, since it spreads the material. Does anyone have any experience with this? Thanks, Rodney
I read it is bad practice to put countersunk screws in plastic, since it spreads the material. Does anyone have any experience with this? Thanks, Rodney
Aug 5, 2004 #2 M MintJulep Mechanical Joined Jun 12, 2003 Messages 10,255 Location JP Depends: On what you are trying to accomplish. On the loads involved. On the type of plastic. Upvote 0 Downvote
Aug 5, 2004 Thread starter #3 rodneyb Mechanical Joined Jun 26, 2001 Messages 30 Location US 0.156" Thick, M3 screw, ABS Plastic. Will be load bearing from Solenoid.. Upvote 0 Downvote