I am researching plasma keyhole welding to apply to Ø 4m X 10mm th. 347SS.
So far I have been told by Plasma Equip suppliers that 10mm is beyond the process capability.
What I have found in text and on the net is very marginal information at best.
I know that this has been done by various companies and in labs.
Does anyone have a contact for someone that is actually using this process or has experience with it.
 
Replies continue below

Recommended for you


for titanium we can weld with keyhole upto 12mm without root gap and bevel but for the stainless steel 10 mm the maximum where you will get better weld and beyond that with bevel preparatio
 