If you are working under ASME then you will have materials identified from the melt source through to the finished installation.
As the work is handed off between parties this information is part of what is required.
You simply don't accept responsibility unless the package is complete.
And you don't wait until the final handoff before raising questions.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed